HTN+CF High Temp CF Nylon 1.75mm Black 500g 3D Printer Filament
HTN+CF High Temp CF Nylon 1.75mm Black 500g 3D Printer Filament

CARBONX™ HTN+CF

SKU: 052BK00A-750G

Regular price
$200.00
Sale price
$200.00
Regular price
$0.00

Benefits of CARBONX™ HTN+CF

  • Reinforced with high-modulus carbon fiber
  • 87 MPa tensile strength and a heat deflection temperature of 240°C
  • Low moisture absorption and superior chemical resistance
  • Excels in high-performance parts, tools, and fixtures
COLOR:
DIAMETER:
REEL SIZE:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

CarbonX HTN+CF

CarbonX™ Carbon Fiber High Temp Nylon (HTN) is engineered for high-strength, heat-resistant applications. Reinforced with high-modulus carbon fiber, it offers 87 MPa tensile strength and a heat deflection temperature of 240°C. With low moisture absorption and superior chemical resistance, it excels in high-performance parts, tools, and fixtures. CarbonX™ HTN+CF provides excellent stiffness and thermal stability, making it ideal for demanding 3D printing projects.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
285°-315 C
140-160°C
Bed Temp
110-120° C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
120C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.