OBSIDIAN™ NYLON 6+CF V2

SKU: 024BK00A-750G

Regular price
$99.99
Sale price
$99.99
Regular price
$0.00
Shipping calculated at checkout.

Benefits of OBSIDIAN™ NYLON 6+CF V2

  • Obsidian™ CF v2 is now a true one-to-one alternative to Markforged’s Onyx
  • Customer tested and approved
  • Bambu AMS compatible
  • Engineered with premium high-modulus carbon fiber and a tough PA6 copolymer base
  • Compatible with a wide range of 3D printers that support PA6+CF materials
  • Strongly recommend this material to be printed through a hardened steel nozzle rather than a softer metal.
Color Code: Black
Diameter:
Reel Size:

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials.

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

OBSIDIAN™ NYLON 6+CF V2

Reformulated. Retested. Remarkable.

When our original Obsidian™ CF didn’t meet expectations on Markforged printers, we took your feedback seriously. We went back to the lab and reengineered the formulation from the ground up: refining the material, enhancing processability, and thoroughly testing to ensure it delivers where it counts.

Obsidian™ CF v2 has undergone extensive in-house testing and real-world validation by our user community. Customers across industries have confirmed exceptional results on Markforged® printers as well as a wide range of open-source systems. From mechanical strength and layer adhesion to surface finish and print reliability, v2 outperforms expectations across the board.

In side-by-side comparisons, Obsidian™ CF v2 is now a true one-to-one alternative to Markforged’s Onyx, but at a better value.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
265-285C
140-160°C
Bed Temp
90-110C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel Nozzle
0.10mm or higher
Layer Height
.10mm or higher
65°C for 4 hours
Drying Specs
80C for 6 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.