Description
CarbonX PEEK+CF20 is one of the premier polymers in FFF/FDM 3D Printing. Made using
20% high-modulus chopped carbon fiber for exceptional stiffness, strength,
and dimensional stability. PEEK+CF20 is one of the highest performance thermoplastics ever invented. It is used in some of the most demanding applications by industries such as Auto, Aerospace, Defense, Semi-conductor, and Oil/Gas. Engineers depend on PEEK for applications where failure is not an option. |
Benefits of CarbonX PEEK+CF20 :
- Superior mechanical properties, even at elevated temperatures
- Excellent chemical resistance
- Low Coefficient of Linear Thermal Expansion (CTE)
- Near Zero moisture absorption
- Low smoke and toxic gas emissions
Reviews
Print Recommendations
![365-390°C](http://www.3dxtech.com/cdn/shop/files/Rec_Extruder__Temp.jpg?v=1718023038&width=100)
Extruder Temp
385-415C
![140-160°C](http://www.3dxtech.com/cdn/shop/files/Rec_Bed_Temp.jpg?v=1718023060&width=100)
Bed Temp
130-150C
![Recommended](http://www.3dxtech.com/cdn/shop/files/Rec_Heated_Chamber.jpg?v=1718023095&width=100)
Heated Chamber
Recommended
![0.4mm diameter minimum](http://www.3dxtech.com/cdn/shop/files/Rec_Nozzle_Specs.jpg?v=1718023127&width=100)
Nozzle Specs
Hardened Steel with .4mm diameter minimum
![0.10mm or higher](http://www.3dxtech.com/cdn/shop/files/Rec_Layer_Height.jpg?v=1718022948&width=100)
Layer Height
0.25mm or higher
![65°C for 4 hours](http://www.3dxtech.com/cdn/shop/files/Rec_Drying_Specs.jpg?v=1718022745&width=100)
Drying Specs
120C for 4 hours
![](http://www.3dxtech.com/cdn/shop/files/Nozzle-Abrasion.png?v=1718882569&width=227)
Abrasive Material
This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.
Because of this, it's strongly recommended this material be printed through a hardened steel nozzle rather than a softer metal. Hardened steel nozzles can often be inexpensive and easily installed depending on your printer manufacturer's instructions.
Material DETAILS
Glass Fiber Reinforced Filament
![](http://www.3dxtech.com/cdn/shop/files/Rectangle111.png?v=1718882852&width=310)
What Is It?
DescriptionFibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament.
This, along with their physical makeup, give this material enormous strength and mechanical properties.
![](http://www.3dxtech.com/cdn/shop/files/Rectangle222.png?v=1718883012&width=310)
What Does It Do?
Glass fiber reinforcement gives material a lot of desirable properties:
High strength
High stiffness
High chemical resistance
Low thermal expansion
![](http://www.3dxtech.com/cdn/shop/files/Rectangle333.png?v=1718883155&width=310)
How Does It Work?
Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.
![](http://www.3dxtech.com/cdn/shop/files/Rectangle444.png?v=1718883273&width=310)
What Is It Good For?
Ideal for any applications which require strength and rigidity.
For these reasons, glass fiber reinforced filament is very popular in automotive, mechanical, civil engineering, and research industries.
RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.