Description
Ecomax® rPETG is
a durable material that has excellent strength while remaining flexible. The
base resin used in our rPETG filament is FDA approved and has improved
chemical resistance compared to PLA or ABS. It is suitable for cleaning with
isopropyl alcohol as needed. |
Benefits of EcoMax R-PETG :
- Superior chemical resistance to ABS
- Very low odor while printing
- Amorphous structure giving it a low, near isotropic shrinkage
- Low moisture absorption, 3x lower than ABS
- Wide range of processing from 230-260°C
- Superior ductility vs. ABS
Reviews
Print Recommendations
![365-390°C](http://www.3dxtech.com/cdn/shop/files/Rec_Extruder__Temp.jpg?v=1718023038&width=100)
Extruder Temp
230-260°C
![140-160°C](http://www.3dxtech.com/cdn/shop/files/Rec_Bed_Temp.jpg?v=1718023060&width=100)
Bed Temp
60-90°C
![Recommended](http://www.3dxtech.com/cdn/shop/files/Rec_Heated_Chamber.jpg?v=1718023095&width=100)
Heated Chamber
Not required
![0.4mm diameter minimum](http://www.3dxtech.com/cdn/shop/files/Rec_Nozzle_Specs.jpg?v=1718023127&width=100)
Nozzle Specs
No special concerns
![0.10mm or higher](http://www.3dxtech.com/cdn/shop/files/Rec_Layer_Height.jpg?v=1718022948&width=100)
Layer Height
No special concerns
![65°C for 4 hours](http://www.3dxtech.com/cdn/shop/files/Rec_Drying_Specs.jpg?v=1718022745&width=100)
Drying Specs
65°C for 4 hours
![](http://www.3dxtech.com/cdn/shop/files/Nozzle-Abrasion.png?v=1718882569&width=227)
Abrasive Material
This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.
Because of this, it's strongly recommended this material be printed through a hardened steel nozzle rather than a softer metal. Hardened steel nozzles can often be inexpensive and easily installed depending on your printer manufacturer's instructions.
Material DETAILS
Glass Fiber Reinforced Filament
![](http://www.3dxtech.com/cdn/shop/files/Rectangle111.png?v=1718882852&width=310)
What Is It?
DescriptionFibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament.
This, along with their physical makeup, give this material enormous strength and mechanical properties.
![](http://www.3dxtech.com/cdn/shop/files/Rectangle222.png?v=1718883012&width=310)
What Does It Do?
Glass fiber reinforcement gives material a lot of desirable properties:
High strength
High stiffness
High chemical resistance
Low thermal expansion
![](http://www.3dxtech.com/cdn/shop/files/Rectangle333.png?v=1718883155&width=310)
How Does It Work?
Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.
![](http://www.3dxtech.com/cdn/shop/files/Rectangle444.png?v=1718883273&width=310)
What Is It Good For?
Ideal for any applications which require strength and rigidity.