TRITON3D™ ABS+CF - Stratasys® Compatible

SKU: ABS03CF200563BK00

Regular price
$75.00
Sale price
$75.00
Regular price
$125.00
Shipping calculated at checkout.

Benefits of TRITON3D™ ABS+CF - Stratasys® Compatible

  • Easier to print than most industrial-grade materials
  • Greatly improved stiffness, modulus, and dimensional stability thanks to the addition of carbon fiber reinforcement
  • Parts can be smoothed with acetone vapors
  • Higher melting point than PLA or PETG
  • Stiff, high-modulus, industrial-grade parts
  • Due to the abrasive nature of carbon fiber, you should anticipate a 50% reduction in tip-life due to higher wear rates vs. unfilled ABS
Color Code: Black
Reel Size:
In Stock

NO. This is big misunderstanding in the 3D printer world. There is actually caselaw and federal statutes (both in the US and Canada) that prevent the manufacturer from invalidating the warranty.  

Learn More

We have purchased Fortus® and Dimension® printers for our in-house evaluation of materials. Please see our compatibility chart on our installation page.

We have also partnered with several large companies who have Stratasys® printers and they have beta tested all of our formulations. We started evaluating materials in late 2015 and launched our first grades June 2017 - so we have a lot of time and effort into assuring these filaments work in your printer. Plus - we have a 100% money back guarantee that should help assure you that we stand behind our products.  

Learn More

Please see our installation guide to learn more. It is very simple and will save you money when you refill your Fortus® or Dimension® with our filaments.  

Learn More

Each spool is carefully produced and packaged to ensure best possible performance in your Stratasys printer. Before you get started, please take a moment to review our Material Handling Instructions to help achieve consistent, high-quality prints.

Learn More

TRITON™ ABS+CF

Triton 3D Carbon Fiber ABS was formulated to be 100% compatible with your Stratasys® printers and come with replacement chips but at a fraction of the cost of Stratasys® brand filament. Refill your Stratasys® printer with our alternative to Carbon Fiber ABS. This grade of CF ABS is 100% guaranteed by Triton 3D® to work in your Stratasys® printers.

TRITON™ ABS+CF is a high-performance carbon fiber reinforced ABS filament ideal for anyone that desires a structural component with high modulus, excellent surface quality, dimensional stability, light weight, and ease of printing. Made using Sabic® MG-94 premium ABS and High-Modulus Carbon Fiber.

We provide the EEPROM chip for your printer (Classic and Plus Style Chip). All you need to do is load your canister, install the chip, and start printing![Canister Loading Instructions]

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
220-240C
140-160°C
Bed Temp
100-110C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
80C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.