ALTRA 280
High-Temperature Performance, Precision, Flexibility
Engineered for large-scale manufacturing, the ALTRA 280 features a rigid welded frame, precision ball screws, and servo-driven motion to maintain accuracy throughout long print jobs. Its expansive 500 × 700 × 800 mm build volume allows users to print bigger parts in a single piece, reducing assembly requirements and improving overall part integrity. This makes it an ideal solution for applications where size, strength, and reliability are critical.
Built for demanding applications
A fully controlled thermal environment allows the ALTRA 280 to process advanced engineering polymers with confidence. With a 180°C heated chamber, 180°C print bed, and DSX extruders reaching up to 450°C, the system ensures optimal layer adhesion and dimensional stability.
Dry Material Storage
A sealed dry-storage chamber keeps filament in optimal condition by preventing moisture absorption. With capacity for two spools, the system ensures materials are always ready for high-quality printing.
KEY FEATURES
Accuracy in Large Scale
Up to 4 DSX Extruders
Fully Automated Quick Start
Even Temperature Distribution
| Dimensions | Temperatures | Key Features |
|---|---|---|
| Size: 74.8" x 65.0" x 76.8" | Nozzle: 450° C | Large Scale Printing |
| Build Volume: 19.7" x 27.6" x 31.5" | Print Bed: 180° C | Open Source Materials |
| Weight: 4365 lbs | Build Chamber: 180° C | Capable to Print PEEK |
MADE FOR ENGINEERING MATERIALS
Let's Talk More About The ALTRA 280