3DXSTAT ESD PLA is an advanced ESD-Safe compound designed for use in critical applications which require electrostatic discharge (ESD) protection. Made using cutting-edge multi-wall carbon nanotube technology, state of the art compounding technology, and precision extrusion processes. Target surface resistance: 10^7 to 10^9 Ohm. |
Print Recommendations

Extruder Temp
210-240C

Bed Temp
23-60C

Heated Chamber
Not required

Nozzle Specs
No special concerns

Layer Height
No special concerns

Drying Specs
65C for 4 hours