Description
This is a
water-soluble support filament based on a new generation of PVA (polyvinyl
alcohol, PVOH). AquaTek™ PVA Water Soluble Support is tap water-soluble and
is easily removed from the printed part with room-temp water. |
Benefits of AquaTek PVA :
- Superior to traditional PVA filament
- Easily soluble in warm water
- Eco-friendly, biodegradable, and safe to dispose in house or office drains
- Ideal support material for the most popular desktop printing materials
Reviews
Print Recommendations
![365-390°C](http://www.3dxtech.com/cdn/shop/files/Rec_Extruder__Temp.jpg?v=1718023038&width=100)
Extruder Temp
190-220C
![140-160°C](http://www.3dxtech.com/cdn/shop/files/Rec_Bed_Temp.jpg?v=1718023060&width=100)
Bed Temp
23-70C
![Recommended](http://www.3dxtech.com/cdn/shop/files/Rec_Heated_Chamber.jpg?v=1718023095&width=100)
Heated Chamber
Not required
![0.4mm diameter minimum](http://www.3dxtech.com/cdn/shop/files/Rec_Nozzle_Specs.jpg?v=1718023127&width=100)
Nozzle Specs
No special concerns
![0.10mm or higher](http://www.3dxtech.com/cdn/shop/files/Rec_Layer_Height.jpg?v=1718022948&width=100)
Layer Height
No special concerns
![65°C for 4 hours](http://www.3dxtech.com/cdn/shop/files/Rec_Drying_Specs.jpg?v=1718022745&width=100)
Drying Specs
65C for 4 hours
![](http://www.3dxtech.com/cdn/shop/files/Nozzle-Abrasion.png?v=1718882569&width=227)
Abrasive Material
This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.
Because of this, it's strongly recommended this material be printed through a hardened steel nozzle rather than a softer metal. Hardened steel nozzles can often be inexpensive and easily installed depending on your printer manufacturer's instructions.
Material DETAILS
Glass Fiber Reinforced Filament
![](http://www.3dxtech.com/cdn/shop/files/Rectangle111.png?v=1718882852&width=310)
What Is It?
DescriptionFibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament.
This, along with their physical makeup, give this material enormous strength and mechanical properties.
![](http://www.3dxtech.com/cdn/shop/files/Rectangle222.png?v=1718883012&width=310)
What Does It Do?
Glass fiber reinforcement gives material a lot of desirable properties:
High strength
High stiffness
High chemical resistance
Low thermal expansion
![](http://www.3dxtech.com/cdn/shop/files/Rectangle333.png?v=1718883155&width=310)
How Does It Work?
Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.
![](http://www.3dxtech.com/cdn/shop/files/Rectangle444.png?v=1718883273&width=310)
What Is It Good For?
Ideal for any applications which require strength and rigidity.
For these reasons, glass fiber reinforced filament is very popular in automotive, mechanical, civil engineering, and research industries.