CarbonX ABS+CF
CarbonX ABS+CF is a high-performance carbon fiber reinforced ABS filament ideal for anyone that desires a structural component with high modulus, excellent surface quality, dimensional stability, light weight, and ease of printing. Made using 10% High-Modulus Carbon Fiber. Made in the USA using premium Sabic MG-94 ABS and premium high modulus carbon fiber.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.


Print Recommendations

Extruder Temp
220-240C

Bed Temp
100-110C

Heated Chamber
Recommended

Nozzle Specs
Hardened Steel with .4mm diameter minimum

Layer Height
0.25mm or higher

Drying Specs
80C for 4 hours
RECOMMENDED