ECOMAX® R-PETG
Ecomax® rPETG is a durable material that has excellent strength while remaining flexible. The base resin used in our rPETG filament has improved chemical resistance compared to PLA or ABS. It is suitable for cleaning with isopropyl alcohol as needed.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations
Extruder Temp
230-260°C
Bed Temp
60-90°C
Heated Chamber
Not required
Nozzle Specs
No special concerns
Layer Height
No special concerns
Drying Specs
65°C for 4 hours
Have a Great Profile? Share It With the Community
Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.
Contact Our Sales Team
Need a larger quantity or looking for a product that's currently out of stock? Complete the form below, and our sales team will reach out to assist with pricing, availability, and purchasing options.
- Choosing a selection results in a full page refresh.