ESD Flex TPU 1.75mm Black 750g 3D Printer Filament
ESD Flex TPU 1.75mm Black 750g 3D Printer Filament

3DXSTAT ESD-FLEX TPU

SKU: TPU02ES200750BK00

Regular price
$135.00
Sale price
$135.00
Regular price
$0.00

Benefits of 3DXSTAT ESD-FLEX TPU

  • High elongation, over 300%
  • Shore 90A semi-flex hardness
  • Ease of printing compared to similar flexible materials
  • Excellent layer bonding
  • Outstanding fatigue resistance
  • Low moisture absorption
  • Retains flexibility even at low temperatures
Color Code: Black
Diameter:
Reel Size:
In Stock

3DXSTAT ESD-FLEX TPU

3DXSTAT ESD-Flex TPU [90A] [thermoplastic polyurethane] elastomer is an engineering-grade thermoplastic chosen for its balance of excellent flexibility, ease of printing, chemical resistance, and toughness. 3DXSTAT ESD Flex elastomeric filament has been formulated to offer ESD-Safe electrical conductivity with a target surface resistance of 10²-10³ Ohm.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
220-240°C
140-160°C
Bed Temp
40-60°C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
65°C for 4 hours
RECOMMENDED